dennisbernal91z
Mechanical
Hi I am new to the forumn and am a product engineer with about 3 years exp.
I am currently haveing a part molded for me that is quite big, it is a case to a medical instrument. It is currently made of ABS+PC (Hybrid S570 or similar) w/ chem. foaming agent (Hydrocerol or sim.). This material is OK, it just looks like white chocolate and the parts needs to be pantone cool gray 1 U.
Here are my questions:
1. How would I spec out a material that can be shot in this color.
2. Is it possible to add dye to the current material?
3. Paint hides sink and mold flow lines, the bare part currently has a lot of these. This would rule out using this material correct?
This is a good start if anyone can help. Thanks so much for any assistance.
-Dennis
I am currently haveing a part molded for me that is quite big, it is a case to a medical instrument. It is currently made of ABS+PC (Hybrid S570 or similar) w/ chem. foaming agent (Hydrocerol or sim.). This material is OK, it just looks like white chocolate and the parts needs to be pantone cool gray 1 U.
Here are my questions:
1. How would I spec out a material that can be shot in this color.
2. Is it possible to add dye to the current material?
3. Paint hides sink and mold flow lines, the bare part currently has a lot of these. This would rule out using this material correct?
This is a good start if anyone can help. Thanks so much for any assistance.
-Dennis