braham0793
Mechanical
Dear ;
Good afternoon,
I will make a line of stainless / Monel 400 pipe, I wonder what suggestions may indicate me to bring good manufacturing process, welding and cleaning.
The line is 3 "and the seals are SW.
The manufacture is for a hydrogen plant.
Best regards.
Good afternoon,
I will make a line of stainless / Monel 400 pipe, I wonder what suggestions may indicate me to bring good manufacturing process, welding and cleaning.
The line is 3 "and the seals are SW.
The manufacture is for a hydrogen plant.