Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SDETERS on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

insulation 1

Status
Not open for further replies.

terry100

Chemical
Oct 3, 2007
6
If i cut a hole in the metal covering of tank insulation to do some ultrasonic testing, what is a good way to seal it until the next round of testing? these are outside tanks
 
Replies continue below

Recommended for you

Why not do the UT inside?
What type of insulation? Aluminium cladding? What's behind the aluminium? How good of a seal do you require? Is the exterior of the tank primed?

<<A good friend will bail you out of jail, but a true friend
will be sitting beside you saying ” Damn that was fun!” - Unknown>>
 
Hopefully not vacuum insulated.... :-D

-handleman, CSWP (The new, easy test)
 
there is chemical in the tanks. it is ceramic fiber with aluminum cladding and i just want to keep rain out
 
Here is the answer to your problem. We use these on all UT access holes especially on tanks and large lines. These serve several purposes, keeping the same location, weather
proof, save making another hole, etc. Studweld is one of several manufacturers.

 