Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Interaction between steel and concrete in ABAQUS

Status
Not open for further replies.

Ali asger

Student
Nov 5, 2024
9
Hello There, I am a student working on abaqus modelling of a composite deck slab for four point bending test as per eurocode 4, i have modelled concrete as solid element , steel as shell element and i have provided boundary conditions using rigid tie constrain the faces of concrete and steel at a node and applying boundary conditions of pinned and roller on two ends , further i have applied surface to surface interaction standard using both normal and tangential behaviour , loading i have apllied using a coupling the load line to a centre point on top of slab and assiging displacement of 15mm , the issue i am facing is that the steel is getting separated from concrete and the bending is not correct as given in image i have attached , how can i fix this please help and further i have seen that by changing the way i am applying the load the initial stiffness of the slab changes i dont know why ? please someone can suggest me how to fix this errors Thankyou



Thankyou
 

Attachments

  • WhatsApp Image 2024-11-06 at 00.26.27_f03d909f.jpg
    WhatsApp Image 2024-11-06 at 00.26.27_f03d909f.jpg
    93.9 KB · Views: 11
Replies continue below

Recommended for you

How did you tie those parts ? On the whole surface or only on the sides ? Some screenshots with the BC/load/constraint symbols would be helpful.
 
Thankyou for your reply sir, please find below attached images , in 1st image i have used rigid tie constrain on the face of concrete as well as steel deck and choose a control point , on that control point i have applied my boundary conditions. In image 2nd i have applied a displacement of 20mm using coupling the loading lines to a center point on top of slab. Hope this will give you a clear idea what i have modeled. Thankyou


Thankyou
 

Attachments

  • WhatsApp Image 2024-11-06 at 11.06.39_0d8a1248.jpg
    WhatsApp Image 2024-11-06 at 11.06.39_0d8a1248.jpg
    107.9 KB · Views: 9
  • WhatsApp Image 2024-11-06 at 11.07.46_9d957ed4.jpg
    WhatsApp Image 2024-11-06 at 11.07.46_9d957ed4.jpg
    165.7 KB · Views: 8
So you don't have a tie constraint - only rigid bodies with tied nodes. You should also apply a tie constraint between the shell and solid if they are supposed to be permanently bonded on the whole interface.
 
i have applied surface to surface contact using penalty friction of 0.5
 
Replace it with tie constraint or tied/cohesive contact if you want them to move together without separating.
 
actually in my case i want to study the slip behaviour of slabs, apart from this actually i rectified i error while using surface to surface interaction and now the steel deck is not getting separated but the slab is unable to predict the initial stiffness correctly , any tips what i should do to correct my results?