Does anyone have a feel for a typical reduction in interlaminar shear strength for a multiaxial laminate as opposed to one made purely of unidirectional plies all at 0 degrees?
Some limited short beam shear data we've got indicates the multiaxial laminate beams could be as little as 60% as strong as 100% 0 degree ones for ILSS. This seemed a bit of a big knockdown.