Guys,
There was ring of rust (corrosion) found at the internal surface of a SS 316L tank at its liquid/air interface. This tank is 3 ft in diameter and 5 ft in height. This tank is above ground standing on three legs on a third floor of a building; it is also connected to piping system, and is grounded. This tank contains a solution of ALPO4 and NaCl with a pH 5.2. I was wondering if catholic protection or sacrificial anode can be used at arrest this corrosion. Please suggest any solution.
Thanks
There was ring of rust (corrosion) found at the internal surface of a SS 316L tank at its liquid/air interface. This tank is 3 ft in diameter and 5 ft in height. This tank is above ground standing on three legs on a third floor of a building; it is also connected to piping system, and is grounded. This tank contains a solution of ALPO4 and NaCl with a pH 5.2. I was wondering if catholic protection or sacrificial anode can be used at arrest this corrosion. Please suggest any solution.