We have a stainless steel ring, that has 30 threaded through holes. Into these holes we place set screws, and the set screws are used to apply a load to an inner ring...used for clamping another machine part.
The ring is stainless, and the set screws are nickel plated. These screws are replaced about two times per week. For the past year we have seen a problem with the internal stainless threads stripping. The screws are 3/8" Diameter. We are applying a maximum of 160in-lbs of torque each time we install these.
So, my questions are:
1. Is there a limit to how many times you can use a threaded hole? Fatigue?
2. Could reducing the torque, by doubling the number of screws solve the problem?
3. Would a different plating or screw material help solve the problem?
4. Any tips on how to solve this problem would be appreciated.
Thanks,
Mike
The ring is stainless, and the set screws are nickel plated. These screws are replaced about two times per week. For the past year we have seen a problem with the internal stainless threads stripping. The screws are 3/8" Diameter. We are applying a maximum of 160in-lbs of torque each time we install these.
So, my questions are:
1. Is there a limit to how many times you can use a threaded hole? Fatigue?
2. Could reducing the torque, by doubling the number of screws solve the problem?
3. Would a different plating or screw material help solve the problem?
4. Any tips on how to solve this problem would be appreciated.
Thanks,
Mike