i have to u a Wire type IQI per ASTM. So selection of essential wire will be on what basis?
Is it on base metal thickness or base metal thickness and allowable reinforcement?

 
Replies continue below

Recommended for you

ASME V Art 2 T-276.2(a) Welds with reinforcement. The thickness on which the IQI is based is the nominal single-wall thickness plus the estimated weld reinforcement not to exceed the maximum allowed by the referencing Code Section.

Both root and cap reinforcecment should be taken into consideration.
 