Is "ASTM A 234 WP12" equal To "AISI 4140"?

thank you
 
Replies continue below

Recommended for you

No, it is not.

Chemically with Chromium and Molybdenum, they are close, but the big difference between the two is the amount of Carbon.

WP12: C = 0.05-0.20%
4140: C = 0.38-0.43%



The devil is in the details; she also wears prada.
 