May 14, 2015 #2 MikeHalloran Mechanical Aug 29, 2003 14,450 0 0 US Grind what? With what? How hot? Why is the surface hot? Mike Halloran Pembroke Pines, FL, USA Upvote 0 Downvote
May 14, 2015 Thread starter #3 james Mechanical May 13, 2015 5 0 0 BT To do grinding after welding in SS (13 Cr 4 Ni) material with SS grinding wheel. The surface temperature will be approximately 100-140 degree centigrade. Upvote 0 Downvote
To do grinding after welding in SS (13 Cr 4 Ni) material with SS grinding wheel. The surface temperature will be approximately 100-140 degree centigrade.