is it advisable to grind in hot surface?
 
Grind what?
With what?
How hot?
Why is the surface hot?


Mike Halloran
Pembroke Pines, FL, USA
 
To do grinding after welding in SS (13 Cr 4 Ni) material with SS grinding wheel. The surface temperature will be approximately 100-140 degree centigrade.
 