Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

is it advisable to grind in Hot Surface?

Status
Not open for further replies.

james

Mechanical
May 13, 2015
5
is it advisable to grind in hot surface?
 
Replies continue below

Recommended for you

Grind what?
With what?
How hot?
Why is the surface hot?


Mike Halloran
Pembroke Pines, FL, USA
 
To do grinding after welding in SS (13 Cr 4 Ni) material with SS grinding wheel. The surface temperature will be approximately 100-140 degree centigrade.
 