Is it necessary to mix accelerator to RCC pavement? 2

Status
Not open for further replies.

bertoS

Civil/Environmental
Aug 9, 2016
9
accelerator, to accelerate the curing process of the RCC.
 
Replies continue below

Recommended for you

Depends on the curing conditions (temperature, humidity, etc) and how soon it needs to be open to traffic
 
most engineers leave it up to the contractor as a means/methods item with the one exception of requiring that all accelerators be non-chloride.
 
Avoid calcium chloride... do you really need to speed things up?

Dik
 