Hello every one, I have one question here. We have a skid package to build. During check the material with MTR. The question is I have a pipe MTR which show ASTM A53 only it not show and other SPEC like ASME. I need A106 GB pipe SPEC ASME or ASTM and we always use it for piping. Is it ok to use ASTM A53B instead of A106B?
 
Replies continue below

Recommended for you

Marsart;
You need to review the ASTM A 53 specification, particularly Grade B. This pipe can be supplied as seamless or welded. ASTM A 106 is seamless pipe for elevated temperature service. You need to look at the mechanical properties between the two specifications and compare.

For example;
A 53 Grade B (Types E and S) 60/35 Ksi UTS/YS
A 106 Grade B 60/35 Ksi UTS/YS
 