Hello,
We have had an issue where a pipe is running through a 150mmx150mm W shaped beam. Is it safe to cut a section (8") of pipe and attach a 100mmx100m W shaped beam below the cut with some overlap? Beam to be attached below cannot be more than 100mm as there is not enough room available. (Please refer to the attached image)
The main beam is simply supported beam of 28' length and having 3 supports between 2 ends. The cut will be at 27" away from one intermediate support on one side and 66" from other support. The beam carries it's self weight and 3 point loads of 0.25kips. One point load of 0.25kips is 4 inch away from the cut.
I'd be grateful for any insight on this. I don't need any detailed examination or anything, just wondering if anyone had seen this done.
We have had an issue where a pipe is running through a 150mmx150mm W shaped beam. Is it safe to cut a section (8") of pipe and attach a 100mmx100m W shaped beam below the cut with some overlap? Beam to be attached below cannot be more than 100mm as there is not enough room available. (Please refer to the attached image)
The main beam is simply supported beam of 28' length and having 3 supports between 2 ends. The cut will be at 27" away from one intermediate support on one side and 66" from other support. The beam carries it's self weight and 3 point loads of 0.25kips. One point load of 0.25kips is 4 inch away from the cut.
I'd be grateful for any insight on this. I don't need any detailed examination or anything, just wondering if anyone had seen this done.