Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Is product analysis required when ladle analysis is provided on MTR? (forged and buttweld fitgs) 1

Status
Not open for further replies.

sgpmi14

Industrial
Joined
Oct 2, 2014
Messages
6
Location
US
I have a customer who is rejecting our MTR's because he states the values on the MTR should be from a product analysis and not from a ladle analysis? I have read ASTM A751 and it states if the heat analysis is lost or inadequate the product analysis is accepted, but it does not state that the product analysis has to be made regardless of the ladle analysis.
Please help me!!
 
Unless his PO stated that he needed a product analyisis, then a heat (melt or ladle) analysis is acceptable per the spec.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Thanks EdStainless ! That helps me out a lot.
 