mak72
Mechanical
- Aug 6, 2009
- 7
Dear All,
I had Radiography Test (RT) for several weld joints and found few are rejected due to porosity. Our Client is insisiting to have more test (we have 5% of the joints) as a penalty of the failure. Is there any penalty on failure of weld joint.
Regards
MAK72
I had Radiography Test (RT) for several weld joints and found few are rejected due to porosity. Our Client is insisiting to have more test (we have 5% of the joints) as a penalty of the failure. Is there any penalty on failure of weld joint.
Regards
MAK72