1.Which ISO welding standard shall be followed for the qualification of welding procedure and welders on Alu Zinc coated steel sheet.

2. Alu Zinc coated and galvanised steel sheet comes under which material group of iso 15608

Thanks
Ganesh
 
Replies continue below

Recommended for you

1. the criminal code.
2. most substrates are low alloy, low strength, like EN 10152 and EN 10346. So usually 1.1, sometimes 1.2. You'll need FM1 certificates.
 