akshayashok
Mechanical
Hi All,
This is my first post to the forum. I am a mechanical engineer designing plastic enclosures for electronic security systems. In a recent project for a plastic enclosure for a remote controller we are seeing cracks starting at specific locations of weld lines. The failure varies from batch to batch but we are trying to find a way to minimize that. Any guidance will greatly help.
I have uploaded one picture with the post and detailed information is below. We have tried and investigated some solutions. preliminary results can be provided by separate email.
The material used: PC-ABS - we can switch to ABS to reduce chances of brittleness of material.
The number of gates used: 1 at the far end south of the big hole. bottom of the remote plastic component in picture.
The gating is on the inside,
There are cams on the inside to make snaps
I have plastic flow contact angle, fill time and weld line location simulations done from our molder in asia.
We tried to use flow tabs to reduce the effect of weld lines as per suggestions on this webpage: and in another document (can be provided by email). But the results vary based on where we connect the flow tab to the main plastic. we need somebody to help us make the decision. The flow tab is being placed inside the large hole.
Please let me know if somebody can help.
With Best regards
Akshay
This is my first post to the forum. I am a mechanical engineer designing plastic enclosures for electronic security systems. In a recent project for a plastic enclosure for a remote controller we are seeing cracks starting at specific locations of weld lines. The failure varies from batch to batch but we are trying to find a way to minimize that. Any guidance will greatly help.
I have uploaded one picture with the post and detailed information is below. We have tried and investigated some solutions. preliminary results can be provided by separate email.
The material used: PC-ABS - we can switch to ABS to reduce chances of brittleness of material.
The number of gates used: 1 at the far end south of the big hole. bottom of the remote plastic component in picture.
The gating is on the inside,
There are cams on the inside to make snaps
I have plastic flow contact angle, fill time and weld line location simulations done from our molder in asia.
We tried to use flow tabs to reduce the effect of weld lines as per suggestions on this webpage: and in another document (can be provided by email). But the results vary based on where we connect the flow tab to the main plastic. we need somebody to help us make the decision. The flow tab is being placed inside the large hole.
Please let me know if somebody can help.
With Best regards
Akshay