Bmechz

Mechanical
Sep 16, 2012
36
ASME sec Viii Div 1 vessel has a dished end formed from a single piece of plate(without any long seam) and the complete vessel is spot radio graphed (joint eff. is 0.85).Kindly let me know whether we can use the joint efficiency 100% for dished end thickness calculation as it seamless.

Baijuz

Baiju Eapen
Static Equipment Design Engineer
 
Replies continue below

Recommended for you

gr2vessels,

This is can be used for non Hemisphercial heads only. Incase of Hemi sphercial heads 0.85 joint efficiency to be used; I just referred the code.
 
If the head is seamless or 100% X-Rayed:

If the Shell-Head circ seam is 100% X-Ray or Modified Spot in accordance with UW-11(a)(5)(b) then the head can have a weld efficiency of 1.00.

If the shell-head seam has Normal Spot X-Ray or no Radiography at all then the head can have a weld efficiency of 0.85.

Modified Spot and Normal Spot are different. I understand if you invoke modified spot you have to X-Ray the T-Section between the Shell logitudinal seam and Shell-Head Circ seam. Do some research. There are are other threads relating to getting a weld efficiency of 1.00 by invoking UW-11(a)(5)(b).

If you decide to have Normal Spot and Modified Spot, then the Modified Spot X-Rays are seperate and in addition to Normal Spot Requirements.

Seamless and 100% X-Rayed heads are treated the same way.
 
brkmech, you are right. I stand corrected.
Cheers,
gr2vessels
 