Hello,
I specified the connection depicted in the first image attached, in which the tension of the plate is transmitted through the web of the column. The fabricator just started to fabricate the connections and i realized that the connection between the plate and web is not good for lamellar tearing. I could use the connection depicted in the second image, but since the fabricator already started to fabricate the connections, i'd like to change the connection only if necessary.
The moment on the connection is not high and the stresses on the plate for the ULS are below the yield stress. The plate is A36(8mm) ,the column is A572(5mm) and the weld will be a 5mm fillet weld. I know that thinner plates are less suscetible to lamellar but this is vague and i wish to know what parameters can be used to determine this susceptibility.
Thank you.
I specified the connection depicted in the first image attached, in which the tension of the plate is transmitted through the web of the column. The fabricator just started to fabricate the connections and i realized that the connection between the plate and web is not good for lamellar tearing. I could use the connection depicted in the second image, but since the fabricator already started to fabricate the connections, i'd like to change the connection only if necessary.
The moment on the connection is not high and the stresses on the plate for the ULS are below the yield stress. The plate is A36(8mm) ,the column is A572(5mm) and the weld will be a 5mm fillet weld. I know that thinner plates are less suscetible to lamellar but this is vague and i wish to know what parameters can be used to determine this susceptibility.
Thank you.