A colleague has a problem and would welcome any experienced advice. He has a large timber dome sports hall - - approx dia is 120 feet height 80 feet. not a true dome - - more the shape of the pointed end of an egg. Built from panels of plywood fixed to heavy wood sections around the edges- - like flanges - - which are then all bolted together. We believe this type is common in USA for storing minerals.
Problem is that after 10 yrs one side is developing a sizeable
and increasing flat area. Somehow it needs to be pushed back into shape and then stiffened so it cannot develop again.

Anyone out there with any experience ??