PersianEng
Mechanical
I am going to specify Cast Iron butterfly valves (4"-84") on a SS316L piping. In order to avoid galvanic corrosion I have specified all valves to be rubber lined on interior surfaces and flange faces with Neoprene to a thickness of 1/8".
1)Are there any potential problems in rubber lining a flange face?
2)Is it practical to rubber line a 84" buttefly valve body?
Thanks
1)Are there any potential problems in rubber lining a flange face?
2)Is it practical to rubber line a 84" buttefly valve body?
Thanks