hiker27
Industrial
- Jun 3, 2013
- 1
- 0
- 0
We have a 2000 watt Mitsubish Laser, we cut ss. Alu and steel. on aluminun we use sheet with a laser film. On the thinner materials this works fine. On 3/16" and thicker, it bubbles or blows the paper. Are there conditions we can use so this does not happen. Our alternative is to use dish soap on the material, this is not cost effective.