1
- #1
I have to create on purpose very small defects (>4mm) on Al stainless steel and 304L welds (by laser welding).The reason for doing that is to check a if a new NDT system can detect them.
The thickness of the samples will be 2, 5 and 10cm.
Do you think that I will be able to creat very small cracks by rapid water cooling after the welding or is there any other way?
The thickness of the samples will be 2, 5 and 10cm.
Do you think that I will be able to creat very small cracks by rapid water cooling after the welding or is there any other way?