Jun 18, 2003 #1 pabasolo Chemical May 10, 2003 16 0 0 UY Any suggestions about usage (or appropriate disposal) of sencondary lead slag? It contains 55% Fe, and 1.5% Pb which makes it a dangerous residue, so disposal is both expensive and complex. thnks