Dear Guys

We have a propylene Heat exchanger with SA179 Killed tubes (no. of tubes 2465 ). Frequent tube leakage has been bothering us in this heat exchanger. Before, I proceed to explain my query, plz see the pressure specs of exchanger ( from construction drawing)

Pressure Shell Side Tube Side

Hydrotest 29.85 kg/cm.2 19.95 Kg/cm.2

Max.allow. 19.95 kg/cm.2 13.31 kg/cm.2
Working press.

Operating pr. 16.19 kg/cm.2 5 kg/cm2 kg/cm.2

With the given parameters, i understand that shell & tubes are hydrotested separately at shop. However, at site while checking tube leaks during the shutdowns.

1. Which is the safe value of pressure testing i shell use for cheking tube leaks during shut downs?

2. What should be the medium of pressure fluid ?

3. Normally we are testing with the propylene available in the shell & use the soap bubble test to chek leaky tube.Is it ok ?

4. If I plan to use Nitrogen for PT, should there be any effect on the pressure values to be used for leak testing ?


Thanks in anticipation
 
ak1965...

In what country is this HX located ?

In what country are YOU located ?

-MJC

 