Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Lexan cement?

Status
Not open for further replies.

twodogs

Electrical
Nov 17, 1999
23
US
A source, please, for a type of optically clear cement to glue 2 pieces of Lexan together. Water-clear, easy process (and cheap!) would be preferred. Thaks-
 
Replies continue below

Recommended for you

Found a sort of answer myself (NASA Tech briefs!) 3M makes an optically clear sheet adhesive. They are very liberal with samples and appl. data. [sig][/sig]
 
try EP30-3 from Master Bond, Inc. in Hackensack New Jersey.
try and get a sample.
its a high temp resistant optically clear low viscosity epoxy adhesive
 