Julia Mahir
Materials
- Dec 21, 2016
- 13
We have one product that currently being produced using extrusion with liquid curing (hot oil).
The end products tend to be sticky. Even with silicon bath to prevent sticky during handling & packaging, eventually the products will still end up stick to one another while in packaging.
We thought it's caused by the products overcured or undercured. We tried adjust the temperature but still sticky.
1) How to determined if one compound is undercured or overcured (reversion)? Any testing?
2) If we were to get rid of the silicon, how to make it non-sticky?
3) any other reason of product being sticky other than it's undercured/overcured?
The end products tend to be sticky. Even with silicon bath to prevent sticky during handling & packaging, eventually the products will still end up stick to one another while in packaging.
We thought it's caused by the products overcured or undercured. We tried adjust the temperature but still sticky.
1) How to determined if one compound is undercured or overcured (reversion)? Any testing?
2) If we were to get rid of the silicon, how to make it non-sticky?
3) any other reason of product being sticky other than it's undercured/overcured?