Lithium and Nickel Metal Hydride

Status
Not open for further replies.

BenCrook

Electrical
Apr 8, 2002
6
I have an application for a rechargeable battery. My question is, which is the better technology--the rechargeable Lithium or the Nickel Metal Hydride? Is one or the other preferable for rechargeability? for current density? for discharge voltage characteristics?
Thanks
 
Replies continue below

Recommended for you

Lithium ion is a 3.6 V system while NiMH is a 1.5 V system (compatible with alkaline batteries). If you have a high energy application, then Li-Ion is the way to go.
With regard to charging and cycle life, NiMH can generally be charged faster and will have longer cycle life than Li-Ion. State of the art charging technology can charge NiMH in about one hour to 80% of capacity and there is technology in development to charge in as little as 15 minutes. Improvements in Li-Ion charging technology have made charging in one hour possible commercially.
 