I would like to ask your opinion about an issue for HC panels.
We have a typical honeycomb panel with orthotropic face sheets . At edges of the panel there is an edge band region (monolithic). This HC panel is attached to a metallic backup structure from these edge band area with only one row of fasteners.
A uniform negative pressure is acting on the panel.
Below I add a simple sketch.
^^^^^^^^^^^^^^^^^^^^^^^^^
IIIIIIIIIIIIIIIIIIIIIIIII
--------------------------------
T \ / T
\ /
---------------------
This pressure load is reacted by heel-toe forces between fastener line and free edge and pull-thru load at fastener line.(If you have Niu's stress analysis and sizing book you can see an example at pages 216 thru 219). OK, up to here no discussion.
1) Are there any bypass loads at the edgeband ? (My opinion is no because there is only one row of fasteners)
2) In Niu's book, without any explanation, %60/%40 rotational restraint is assumed for ramp & fastener ends, respectively. As engineers, we love this magic number (60/40) but what is the justification of it?
Thanks in advance.