Someone knows if there is some restriction on ASME Section VIII Div.1 or in other part of BPVC, when I have to joint two Course of Pressure Vessel, is possible to have the longitudinal joints of the Course on the same axis ? the picture is attached.

Sorry for my English and thank you for your help.

Flaiano
 
 http://files.engineering.com/getfile.aspx?folder=0a2f0726-37de-41a3-a996-911077b7a6c8&file=DWG.png
Replies continue below

Recommended for you

Flaiano, there are RT restirctions on your option 2. See UW-9(d). I'd consider it poor practice, in any case.

Regards,

Mike
 
Thank You very much Mike, your help saves me a lot of time.
Best Regards
Flaiano
 