afarboudi
Mechanical
- Sep 22, 2015
- 14
Hi everybody
we have faced with a problem that longitudinal weld of some fittings (i.e two elbows or two reducer) are along side of each other.
the design code is B31.3 and it does not have any clause about this matter that it is prohibited or not. on the other side we are in construction and the piping designers do not want to change or modify something.
what NDT we can do and also PWHT is required or not?
*the material is C.S
we have faced with a problem that longitudinal weld of some fittings (i.e two elbows or two reducer) are along side of each other.
the design code is B31.3 and it does not have any clause about this matter that it is prohibited or not. on the other side we are in construction and the piping designers do not want to change or modify something.
what NDT we can do and also PWHT is required or not?
*the material is C.S