Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Looking for 1956 ASME Section II allowables for A212A and A212B (or a nearby year).

Status
Not open for further replies.

22west

Mechanical
Oct 31, 2002
80
Hi,

I am looking to see if anyone has a 1956 copy of ASME Section II where they could look up and tell me the published allowable stresses for both A212A and A212B firebox steels.
I would also take something "in the vicinity" of 1956 as well.

Thanks,
22west
 
Replies continue below

Recommended for you

According to the 1950 edition of section VIII the allowable up to 650°F was 16.25 ksi and 17.5 ksi, for SA-212 grade A and B, respectively. This is based on a design margin on ultimate of 4.
 