Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Looking for correct weld callout

Status
Not open for further replies.

aldumoul

Mechanical
May 24, 2011
65
Currently, this is called out as a Spot weld. I don't think this is correct. This is basically a tack weld. I want to use symbology and not call it out as "4X Tack Weld." It is used to hold the parts together for shipping/assembly purposes.

Thanks,
Alan
 
Replies continue below

Recommended for you

If the weld is ultimately a fillet, it should be a weld symbol with a fillet triangle and a tail with text in it that states TACK.

 
The basic welding symbol consists of a reference line and an arrow. That welding symbols essentially says, "weld here" without defining the type of weld required, i.e., fillet, groove, plug, slot, etc. Any additional information simply adds more information and direction for the welder.

There is nothing wrong with specifying the tack weld as fillet welds of a certain size and length if that is what is required. The detailer can use multiple reference lines as a means of specifying the tack weld on the reference nearest the arrow and the required production weld on the second reference line. A reference in the tail can direct the reader to a note that tells the welder when the final production weld is made. If the tack weld is used to hold members in alignment for subsequent match drilling and bolting or machining for example, all that is needed a single reference line with the appropriate weld symbol (weld type), size, and length is all that is necessary.

Welding symbols with multiple reference lines are useful to designate the sequence of operations and can combine welding and NDT requirements in a single combined welding/NDT symbol.


Additional information on the subject can be found in AWS A2.4 Standard Symbols for Welding, Brazing, and Nondestructive Examination. Every professional should have access to the latest edition of A2.4. Other reference sources usually have information on welding symbols that is outdated. I saw one, I will not say which one it was, but I will say it was recently purchased and it listed welding symbols that were 30 years out of date.


Best regards - Al
 