EdStainless
Materials
- May 20, 2004
- 16,305
We supply cold drawn 304 tubing. In the cold drawn condition the yield strength is roughly 110ksi (UTS 140ksi) and the hardness is about 30RC. The inside surface finish is 25microinches. Just for discussion let's say that the size is 1.000" od x 0.025" wall.
I have a customer that wants the inside surface harder for wear resistance reasons.
Limits, you bet. The outside should not get hardened. The id surface must not get rough. The id tolerance +/-0.002".
I have thought about EN plating, but that would also require a hone to finish.
Ion-nitriding would probably cause too much distortion.
Any thoughts? What have you seen out there that looks interesting?
= = = = = = = = = = = = = = = = = = = =
Corrosion never sleeps, but it can be managed.
I have a customer that wants the inside surface harder for wear resistance reasons.
Limits, you bet. The outside should not get hardened. The id surface must not get rough. The id tolerance +/-0.002".
I have thought about EN plating, but that would also require a hone to finish.
Ion-nitriding would probably cause too much distortion.
Any thoughts? What have you seen out there that looks interesting?
= = = = = = = = = = = = = = = = = = = =
Corrosion never sleeps, but it can be managed.