aegis4048
Petroleum
- Apr 23, 2024
- 35
Hi, I'm seeing two kinds of P&IDs for primary separators from wellhead:
1) PSV venting to air
----> Safer, because it's always guaranteed to work (almost always). But its "dirtier"
2) PSV relieving to flare line
----> Cleaner, but if something goes wrong with flare line, HP shutdown will have to be triggered, resulting in downtime.
I see well sites, some with option 1, and some with option 2. I asked this question to my supervisor and he just told me to go with option 1 because its safer, and that "it's only the big companies that have that one nerd guy that only does these P&ID things that choose to implement these fancy-pants things."
What are yall's thoughts on this? If I am to be tasked with PSV design in the future, what should I implement?
1) PSV venting to air
----> Safer, because it's always guaranteed to work (almost always). But its "dirtier"
2) PSV relieving to flare line
----> Cleaner, but if something goes wrong with flare line, HP shutdown will have to be triggered, resulting in downtime.
I see well sites, some with option 1, and some with option 2. I asked this question to my supervisor and he just told me to go with option 1 because its safer, and that "it's only the big companies that have that one nerd guy that only does these P&ID things that choose to implement these fancy-pants things."
What are yall's thoughts on this? If I am to be tasked with PSV design in the future, what should I implement?