Hi,

I'm machining threads on to the ends of chrome rod for use in hydraulic rams.
I have a ram which will see a maximum retracting load of 10 ton (98.1kN). For this I'm considering a thread of M30x2mm pitch. The chrome rod we use has a tensile strength of 550 n/mm2 with a yielding of 420 n/mm2.

What is the best way to calculate max loading in newtons that the thread can be subjected to before snapping?

Thanks
 
Replies continue below

Recommended for you

Where can I get a copy of these codes?
Is there literature readily available that contain standard calculations for engineers for this calculation?
 
well usually codes you have to buy...
you might find copy using google
lots of free literature on that subject ....depending what part of the world you are
 
Your Mechanical Engineer's Handbook not available?
Got to invest in something!
 
There are a boatload of online calculators easily accessible by a simple google search.

It is better to have enough ideas for some of them to be wrong, than to be always right by having no ideas at all.
 
Typically I design to ~80% of yield for threads that will need to be reused often in the future, 90%+ for threads on parts like cylinders that rarely need to be taken apart.
 