Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Machine-ability for EN10025 S355JO 2

Status
Not open for further replies.

Papax4

Mechanical
Jul 30, 2008
1
Does anyone have machining experience for this material. I need to know suggested surface footage and some sort of machineability rating.

Thanks
 
Replies continue below

Recommended for you

S355J0 is a common unalloyed steel with a yield of min. 355MPa and charpy's at 0°C (J0). It is comparable to A572 grade 50. Machining shouldn't pose a problem.
 
Find a low carbon steel (< 0.20% C) on one of the machinability rating tables from Sandvik, etc. This is not a free-machining grade, but it is easily machined.
 