5,628
We routinely rebuild Pulverizer/bowl Mill "journals."

Two of the grinding rolls/tires we received last week have curious features in the bores.
Instead of the two typical smooth bands with a relief in the middle, these rolls have what look to be serrations cast in the bands.

I'm thinking if a cutting tool is used to "hard turn" the finished roll bores those serrations would make a horribly interrupted cut.

Maybe if that roll OEM grinds the finished bores having to remove only about 50% as much material is a benefit.

Has anyone seen similar details in difficult to machine materials.
 
 https://files.engineering.com/getfile.aspx?folder=2df344a0-2b4e-4d1c-a1b5-6e911fa4e6c2&file=Roll_A_and_C_bore_DSC00368_shrink_and_crop_medlye_.jpg
Replies continue below

Recommended for you

Status
Not open for further replies.

Part and Inventory Search

Sponsor