I started this job early this year. They have most parts machined with a note on the drawing "All dimensions are after plating". Majority of plating is nom .0005.
If I were machining the parts, I use CAM and deduct this amount.
I'm curious how would others do it? I'm trying to reduce cost and errors.
Thanks.
ctopher, CSWP