Wе have developed the technology of fabrication of complex shapes items from cermet TiC-(Ni-alloy) for use at temperatures up to 1000 C.
We must select the incisors for turning.
Experiments have shown that the incisors of cubic boron nitride, of diamond composites (content diamond 70%) quickly crumble and wear - photo attached.
Cermet TiC-(Ni-alloy) have heterogeneous structure and consists of grains of solid titanium carbide, located in a soft metallic matrix - photo attached.
Is possible rapid grinding with diamond wheels. The grain should be at least 0,35-0,50 mm.
However, for complex shapes, such as balls and seats ball valves (have spherical surface) need special grinding machines and tools.
Therefore, for turning workpieces on conventional lathes and machining centers need wear-resistant inserts (incisors).
Thank you in advance for your advice, suggestions and information.
Wе have developed the technology of fabrication of complex shapes items from cermet TiC-(Ni-alloy) for use at temperatures up to 1000 C.
We must select the incisors for turning.
Experiments have shown that the incisors of cubic boron nitride, of diamond composites (content diamond 70%) quickly crumble and wear - photo attached.
Cermet TiC-(Ni-alloy) have heterogeneous structure and consists of grains of solid titanium carbide, located in a soft metallic matrix - photo attached.
Is possible rapid grinding with diamond wheels. The grain should be at least 0,35-0,50 mm.
However, for complex shapes, such as balls and seats ball valves (have spherical surface) need special grinding machines and tools.
Therefore, for turning workpieces on conventional lathes and machining centers need wear-resistant inserts (incisors).
Thank you in advance for your advice, suggestions and information.