Does someone know the hardness (Vickers, Brinell...) of the magnesium alloy AMS4439 or does someone know a good site or book to find tables of hardness for magnesium alloys.

Thanks

Adam
 
Replies continue below

Recommended for you

MIL-HDBK-5J which brings the data from the AMS onlyspecify tensile and compressive values. Hardness is not guaratied same as with PH steels.
 
Aeroad...

MS4439E provides hardness test requirements... and defines what they mean. See AMS4439 Para 8.3...

Regards, Wil Taylor
 