Is there a reference that defines a category for a magnetic permeability of 2.0? I understand the comparison to air=1.0, but it would be helpful if this could be described as "nonmagnetic".
eg: for review of CRES fasteners (MS24694C) to install near to a magnetic flux valve.
Thanks for your help.
eg: for review of CRES fasteners (MS24694C) to install near to a magnetic flux valve.
Thanks for your help.