Hi

I am designing a solenoid to interact with a magnetite-powder tip. I can't find specifications about the magnetite I am using, and properties seem to depend on factors I don't know. Could you give me a rough estimate (just order of magnitude is fine) of the force given a certain magnetic field B of the solenoid and a tip of area pi*(0.2mm)^2 covered in magnetite powder?

Thank you
Cristina
 
Replies continue below

Recommended for you

since the permeability of magnetite is hundreds (if not thousands) of times higher than air, you can treat it as steel. in this case, the pulling force F = .577 x B^2 x S
B- the flux density at the magnetite tip (not the B inside the solnoid which should be larger than B at a distance to the tip), unit: KG
S-area of tip in square inch
F - force in lb
Assuming B = 5kG, F = .577 x 5x5 x 3.14 (.2/25.4)^2 = .0028 lb