Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Making silicone bladder for composite molding

Status
Not open for further replies.

ingear

Mechanical
Jul 27, 2010
2
I've seen several good posts on composite bladder molding, but I'm wondering if anyone has some specific recommendations for:

1) Silicone materials, sources, methods to use to make the bladders
2) Wall thickness of the bladder

FYI we can't used a trapped solid rubber mandrel since it would be trapped in the mold due to the bends in the part.

Thanks
 
Replies continue below

Recommended for you

I once saw a college club use a bicycle tube as their bladder. It was for a one off part but it worked quite effectively, squeezing out a decent amount of resin. What is the diameter of the part you're trying to make?

 
Thanks, I've heard about that. My part is about 0.75" in diameter, but varies.

I suppose was post was a little vague, but I was just wondering if there are rules of thumb for building bladders. We'll experiment with some silicone molds.
 
One important thing is to make sure that your bladder is more or less circular when inflated. Uneven shape = uneven pressure = uneven resin content. You can try getting a inner bladder that about the same size as the outside tube but then you run the risk of folds in your material. If you can try picking a bladder that stretches some so you can vary the pressure and have nice flat surface

 
Ingear,

Try the silicone from Smooth-On. They are at I have used the silicone that they specify for moulding as well as their dragon skins 10 minute. The ten minute is colorless and quite elastic but does run a little bit. The material for mould making is green and more stiff. Either of these can be sprayed or brushed as well as injected into a mould using an epoxy gun to make a tube. I have used with epoxy and polyester, vinyl ester and they work fine.

Good Luck

Mike
 