Hi,
Only the three fabrication methods showed in the document below are permitted?
A fabricator want to fabricate a rectangular HSS by welding two plates (rolled in L section) in two corners of final HSS.
Thanks,
Daniel
Only the three fabrication methods showed in the document below are permitted?
A fabricator want to fabricate a rectangular HSS by welding two plates (rolled in L section) in two corners of final HSS.
Thanks,
Daniel