Hi friends,
I have a part which it's material is 17-4PH ss and H1025 condition is requested. I know after H1025 the hardness might up to 38HRc. So I have to leave it the last step. I have 2 questions below :
1. Is it a necessary step to apply solution condition A before H1025? What might happen if the material I bought has no condition A and I send it to H1025 directly?
2. I have manufacturing procedure options I and II listed below. Could someone kindly give me some suggestion about which one is correct?
Option I :
17-4 plate -> Condition A (1900°F, air cool below 90°F) -> Machining -> H1025
Option II :
17-4 plate -> Machining -> Condition A (1900°F, air cool below 90°F) -> H1025
Thank you for your kindly help.
I have a part which it's material is 17-4PH ss and H1025 condition is requested. I know after H1025 the hardness might up to 38HRc. So I have to leave it the last step. I have 2 questions below :
1. Is it a necessary step to apply solution condition A before H1025? What might happen if the material I bought has no condition A and I send it to H1025 directly?
2. I have manufacturing procedure options I and II listed below. Could someone kindly give me some suggestion about which one is correct?
Option I :
17-4 plate -> Condition A (1900°F, air cool below 90°F) -> Machining -> H1025
Option II :
17-4 plate -> Machining -> Condition A (1900°F, air cool below 90°F) -> H1025
Thank you for your kindly help.