Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Marking change in elevation

Status
Not open for further replies.

Manfreds2

Mechanical
Jan 9, 2008
12
We are installing raised platforms and need to have some sort of yellow marking around the edge to show that there is a change in eleveation. It needs to me something that can be installed, not painted, and the idea of a sticker has been thrown out.

The platform material is fiberglass and about 2" thick.

Any suggestions would be great, thanks!

schreyer2@gmail.com
 
Replies continue below

Recommended for you

Thanks to everyone, you've been very helpful!
 