I have a client who asked me to look at an existing building that has developed some cracks. The customer is concerned that the cracks pose a structural risk to the building.
The building was constructed 11 years ago. The building is 100’ wide x 200’ long x 26’ tall steel framed with 8” masonry walls used as infill. I visited the site over the weekend and took a few pictures. The building is oriented in such a way that the 200’ side faces the east and west direction. Some of the cracks (which have already been repaired) occur on the each 200’ long side but not the 100’ long sides.
A few things I noticed:
-Masonry contraction joints are at 40’ o.c..
-no visible contraction joints were observed in the foundation wall (only construction joints).
-Masonry joints do not align with construction joints.
-Cracks are concentrated at the bottom 3-4 courses of masonry and are above foundation cracks.
-The building is constructed in an area that tends to have a lot of sand (I don’t know this for certain).
The cracks almost look like shrinkage cracks…..but the building has been in place for 11 years so unless the cracks are just opening up now…. Or nobody ever saw them before, I don’t know.
Does anyone have any idea on what the cracks might be cause by?
The building was constructed 11 years ago. The building is 100’ wide x 200’ long x 26’ tall steel framed with 8” masonry walls used as infill. I visited the site over the weekend and took a few pictures. The building is oriented in such a way that the 200’ side faces the east and west direction. Some of the cracks (which have already been repaired) occur on the each 200’ long side but not the 100’ long sides.
A few things I noticed:
-Masonry contraction joints are at 40’ o.c..
-no visible contraction joints were observed in the foundation wall (only construction joints).
-Masonry joints do not align with construction joints.
-Cracks are concentrated at the bottom 3-4 courses of masonry and are above foundation cracks.
-The building is constructed in an area that tends to have a lot of sand (I don’t know this for certain).
The cracks almost look like shrinkage cracks…..but the building has been in place for 11 years so unless the cracks are just opening up now…. Or nobody ever saw them before, I don’t know.
Does anyone have any idea on what the cracks might be cause by?